PROJECT 70 182-FM is a ferritic free-machining stainless steel designed to have machinability approaching that of AISI Type 416 stainless steel with corrosion resistance comparable to AISI Type 303 stainless steel. It is ideally suited for automatic screw machines and can be used for many of the same applications as Type 303. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-334. Producer or source: Carpenter.