Abstract

TECHALLOY C (62-16) is a nickel-chromium-iron electrical resistance alloy for operating temperatures up to 1700 F. It can withstand high overloads; this makes it ideal for heavy-duty rheostats and controls. It is highly suitable for heating elements in domestic appliances. It's high electrical resistance and high strength in small sizes make it very useful where space is a factor. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-219. Producer or source: Techalloy Company Inc..