Abstract

UNILOY 18-2 FM is a ferritic stainless steel designed to offer an optimum combination of machinability and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-312. Producer or source: Cyclops.