Abstract

AMPCOLOY 910 is copper containing 0.12% zirconium. It retains high conductivity with good strength, hardness and ductility at elevated temperatures. It is used in a variety of applications such as collector rings, current-carrying shafts and bearings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-295. Producer or source: Ampco Metal Inc..