Abstract

Copper Alloy No. 954 is a copper-aluminum-iron alloy characterized by high strength and hardness, good resistance to fatigue and wear, and excellent corrosion resistance. It is suited for service up to 750 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-292. Producer or source: Copper alloy foundries.