Abstract

Copper Alloy NO. 182 is an age-hardening type of alloy that combines relatively high electrical conductivity with good strength and hardness. It was formerly known as Chromium Copper and its applications include such uses as resistance-welding-machine electrodes, switch contacts and cable connectors. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-305. Producer or source: Copper and copper alloy mills.