Abstract

Nickel-Copper Alloys 410 and 411 are strong and ductile casting alloys; they are generally used in conjunction with wrought counterparts. They can be cast readily into fittings such as elbows, tees, return bends, flanges and similar components. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-214. Producer or source: Nickel alloy casting producers.