Abstract

FERRO-TIC HT-6 is comprised of a dispersion of extremely hard, inert titanium carbide grains in a precipitation-hardenable, nickel-base matrix. It provides a combination of oxidation, corrosion and wear resistance unavailable in other materials for tools and many other uses. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as creep. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, surface treatment, and powder metal forms. Filing Code: Ni-207. Producer or source: Chromalloy American Corporation.