Abstract
Copper No. 101 is a wrought oxygen-free, high-conductivity copper for electrical and electronic applications. Its trade designation is OFE (Oxygen Free Electronic) copper. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-278. Producer or source: Copper and copper alloy mills.
chemical composition, Copper alloy no. 101, corrosion-resistant alloys, elasticity, electrical applications, electronic applications, fatigue properties, fracture toughness, hardness, heat treatability, joinability, low-temperature alloys, machinability, oxygen-free copper, physical properties, shear strength, tensile properties, workability, wrought copper alloys
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Electrical and electronics
Corrosion-resistant alloys
Oxygen-free copper
Wrought copper alloys
Copper alloys
Chemical composition
Heat treatability
Joinability
Machinability
Workability
Elastic modulus
Fatigue properties
Fracture toughness
Hardness
Shear strength
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.