AMDRY 755 is a nickel-base alloy designed to provide good resistance to combinations of abrasion, corrosion, impact, heat and oxidation. The alloy has good machinability characteristics and is easier to machine than AMDRY 756. It is deposited by spraying on the desired surface at a thickness usually limited to a maximum of 0.080 inch. The data pertain to the deposit after fusing. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and powder metal forms. Filing Code: Ni-204. Producer or source: Alloy Metals Inc..