Abstract
L.T.C. is a gold-nickel-chromium solid-solution alloy developed to meet the need for an improved winding wire for potentiometers of utmost reliability. It is characterized by excellent corrosion resistance combined with an unusually low temperature coefficient of electrical resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: Au-2. Producer or source: Sigmund Cohn Corporation.