FEDERATED F410 is a heat-treatable aluminum sand casting alloy recommended for uses requiring high strength along with toughness and ductility. It has good machinability, fair castability, and is suitable for a number of automotive and aerospace applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-210. Producer or source: Federated Metals Corporation, ASARCO Inc..