Abstract
INCOLOY alloy 903 is a precipitation hardenable nickel-iron-cobalt alloy whose outstanding characteristics are a constant low coefficient of thermal expansion, a constant modulus of elasticity and high strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-50. Producer or source: Huntington Alloy Products Division, An INCO Company.