Abstract

UHB Stainless 44L is a high-strength, corrosion-resistant steel with a duplex structure of about 40% austenite in a ferrite matrix. It is produced with extra-low carbon content for good weldability and good resistance to embrittlement and corrosion induced by carbide precipitation. It has excellent stress-corrosion resistance and an optimum combination of strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-288. Producer or source: Uddeholm Aktiebolag.