Abstract

PYROMET 718 is an alloy designed to display exceptionally high yeild, tensile and stress-rupture properties at temperatures up to 1300 F. (704 C). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-193. Producer or source: Carpenter Technology Corporation.