Abstract

CRUCIBLE VERSASTEEL is a type of tool steel with its composition carefully balanced to provide an unusual combination of fine grain structure, high secondary hardness and compressive yield strength, good toughness and exceptional wear resistance. Its resistance to tempering approaches that of high-speed steels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-256. Producer or source: Crucible Specialty Metals Division, Colt Industries.