Abstract

PYROMET 90 is a precipitation-hardenable nickel-base alloy with high strength at high temperatures. It is highly resistant to oxidation, scaling, heat and corrosion. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-192. Producer or source: Carpenter Technology Corporation.