KORLOY 3130 and 3330 are wrought zinc-base alloys with good strength and ductility. They are easily forged, extruded and machined. They are dimensionally stable, have excellent creep characteristics and offer unusual resistance to grain growth at elevated temperaturess. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zn-15. Producer or source: Cominco Ltd.