Abstract

FERRO-TIC CM is a cemented carbide comprising titanium carbide in a matrix of high-chromium tool steel. It is machinable and heat treatable by conventional means, and is recommended for heavy stamping or forming tools and wear-resistant components. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as heat treating, machining, joining, and surface treatment. Filing Code: TS-253. Producer or source: Chromalloy American Corporation, Sintercast Division.