AISI 8625 is a triple-alloy steel of moderate hardenability. It is suitable for many engineering applications when normalized or quenched and tempered. It is also used in the carburized condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-287. Producer or source: Alloy steel mills and foundries.