Abstract

IN-787 is an age-hardenable, high-strength structural steel. It is characterized by low-temperature toughness, good atmospheric corrosion resistance and excellent weldability, even under adverse field conditions such as line-pipe welding. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-286. Producer or source: International Nickel Company Inc..