Abstract

SuperSilverCopper-155 is a silver-bearing deoxidized copper that has excellent electrical conductivity and a high softening point. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-267. Producer or source: Copper Range Company.