CARPENTER VACUMELTROL 41 is a precipitation-hardenable alloy designed for severely stressed high-temperature applications. It possesses high strength in the 1200-1800 F temperature range. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-197. Producer or source: Carpenter.