Abstract

AMAX-MZC is a copper-magnesium-zirconium-chromium alloy in which good electrical conductivity, a high softening point, and good mechanical properties can be achieved by aging without the requirement of a previous solution heat treatment. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-265. Producer or source: Amax Copper Inc..