Abstract
UDIMET 105 is a nickel-base alloy which was developed for service at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-175. Producer or source: Special Metals Corporation.