Abstract

Ti-35A and Ti-50A are commercially pure titanium grades with guaranteed minimum tensile strengths of 35000 psi and 50,000 psi, respectively. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-65. Producer or source: Titanium Metals Corporation of America.