Abstract

EMPIRE ISO-450 is a cast stainless steel with excellent corrosion resistance. A simple, single-step aging treatment develops high strength with good ductility and toughness. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-273. Producer or source: Empire Steel Castings Inc..