Abstract
COPPER ALLOY No. 210 is a 5% zinc brass having excellent cold working properties. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-255. Producer or source: Brass mills.