Abstract

UDIMET 75 is a nickel-base high-temperature alloy developed for good resistance to oxidation and scaling to 2000 F. It can be fabricated and welded readily. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-171. Producer or source: Special Metals Corporation.