Abstract
AISI 1025 is a low-to-medium-carbon steel used in the hot-worked, cold-worked, normalized or water-quenched-and-tempered condition for general-purpose construction and engineering. It is also used for case-hardened components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CS-47. Producer or source: Carbon and alloy steel mills.