TITANALOY is a zinc-base alloy containing copper and titanium. It can be readily formed, joined, and finished and is stronger and more dent resistant than the more common zinc alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Zn-13. Producer or source: Matthiessen & Hegeler Zinc Company.