BLENDALLOY 22-1000 is a high-purity nickel for use where low base hardness, high, ductility, and a low work-hardening rate combined with product purity, corrosion resistance, heat dissipation, electrical conductivity and formability considerations are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-183. Producer or source: Spang Industries Inc..