PD-135 is an oxygen-free, age-hardenable copper containing chromium and cadmium. It has excellent mechanical properties and high electrical and thermal conductivities. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-261. Producer or source: Phelps Dodge Copper Products Company.