LODEX ALLOYS 30 to 43 are a series of permanent magnet alloys which can be held to close magnetic and physical tolerances. This datasheet provides information on composition and physical properties. Filing Code: Co-66. Producer or source: General Electric Company, Magnetic Materials Section.