Abstract

UNILOY 302-HQ is an austenitic stainless steel designed to be used for cold forming with minimum force and maximum deformation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-257. Producer or source: Cyclops.