Abstract

HYTEMCO is a nickel-iron alloy with a high temperature coefficient of electrical resistance. It is recommended for electrical instruments and controls, such as ballistic devices and resistance thermometers, operating in air up to 1100 F. This datasheet provides information on composition, physical properties, and tensile properties. Filing Code: Ni-165. Producer or source: Driver-Harris Company.