Abstract

ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmagnetic even after severe cold work. Common applications are in the petrochemical, chemical, pulp and paper, textile, food processing, and marine industries. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-252. Producer or source: Armco Steel Corporation, Advanced Materials Division.