Abstract

PYROTOOL W has been designed to possess high strength and hardness at temperatures up to 1500 F (816 C). Applications include high-temperature tooling, extrusion dies, dummy blocks, rings, holders, forging dies and mandrels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-161. Producer or source: Carpenter Technology Corporation.