Abstract

BRONWITE is a low-melting, white-bronze, nickel-free casting alloy which was developed as a replacement for nickel silver and other white casting alloys containing nickel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-227. Producer or source: Federated Metals Corporation, ASARCO Inc..