Abstract
ARMCO 410 Cb is a modification of Type 410 stainless steel which combines greater ease of heat treatment with increased strength and toughness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-261. Producer or source: Armco Steel Corporation, Advanced Materials Division. See also Alloy Digest SS-145, July 1963.
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Martensitic stainless steel
Corrosion-resistant alloys
High-temperature alloys
Chemical composition
Heat treatability
Joinability
Machinability
Workability
Creep properties
Elastic modulus
Fatigue properties
Fracture toughness
Hardness
Tensile properties
Physical properties
Thermal properties