AWX STEEL is a columbium-bearing low-alloy steel supplied at four yield strength levels where excellent formability and good weldability are required and corrosion resistance is not a great factor. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-269. Producer or source: Alan Wood Steel Company.