ENDURO AA is a ductile, non-hardening alloy containing 14 to 18 percent chromium with carbon under 0.12 per cent. It has mechanical properties equal to high grade medium carbon steel, with high resistance to general corrosion and oxidation at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-9. Producer or source: Republic Steel Corporation.
ENDURO AA, corrosion-resistant alloys, oxidation resistance, chemical composition, creep properties, elasticity, fatigue properties, fracture toughness, hardness, tensile properties, physical properties, workability, heat treatability, machinability, joinability, high-temperature alloys, low-temperature alloys
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Stainless steel
Corrosion-resistant alloys
High-temperature alloys
Chemical composition
Oxidation resistance
Heat treatability
Joinability
Machinability
Workability
Creep properties
Elastic modulus
Fatigue properties
Fracture toughness
Hardness
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.