Abstract

UNICUT is a molybdenum-tungsten type of high-speed steel containing relatively high percentages of carbon and vanadium. It possesses extremely high edge strength at high hardnesses. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-14. Producer or source: Cyclops Corporation.