Abstract
Silvaloy 355 is a low melting, free-flowing silver brazing alloy recommended for ferrous and nonferrous metals. It is cadmium free, highly ductile, corrosion resistant, and has a nearly white color. This datasheet provides information on composition, physical properties, and shear strength. It also includes information on joining. Filing Code: Ag-1. Producer or source: The American Platinum Works.