Abstract
GRAPH-M.N.S. is an air or oil hardening steel containing free graphite. In the hardened condition it has high resistance to scuffing, galling and seizing. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming and heat treating. Filing Code: TS-13. Producer or source: Timken Roller Bearing Company.