Abstract

ABK Metal is a nickel-chromium cast iron with excellent wear resistance, recommended for severe abrasive service. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on wear resistance as well as casting, heat treating, machining, and joining. Filing Code: CI-4. Producer or source: American Brake Shoe Company.