Abstract

Chase TELNIC BRONZE is a high strength copper-base alloy, hardenable both by heat treatment and cold work, and also having good conductivity, corrosion resistance, cold and hot workability, and excellent machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-4. Producer or source: Chase Brass & Copper Company Inc..