UNILOY 326 is a two-phase, ferromagnetic stainless steel characterized by high strength and very good general and stress corrosion resistance. It has distinct advantage for the fastener industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-241. Producer or source: Cyclops.