INCOLOY ALLOY 802 is a high-carbon iron-base alloy recommended for high-temperature applications requiring excellent corrosion resistance and good mechanical properties. It is furnished in the annealed condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-240. Producer or source: Huntington Alloy Products Division, An INCO Company.