Abstract

ARCASI 67 is an aluminum-zinc-magnesium casting alloy capable of developing high strength by artificial aging. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Al-197. Producer or source: Arwood Corporation.